This search combines search strings from the content search (i.e. "Full Text", "Author", "Title", "Abstract", or "Keywords") with "Article Type" and "Publication Date Range" using the AND operator.
Beilstein J. Nanotechnol. 2014, 5, 2007–2015, doi:10.3762/bjnano.5.209
Figure 1: Left: ZnO-NP prepared by the acidic procedure (sample 1, without labelling; scale bar: 50 nm). Righ...
Figure 2: TEM pictures of ZnO-NP 1 (labeled with a perylene dye) as prepared (left) and after one hour of rea...
Figure 3: Left: TEM picture of degraded ZnO-NP 2 (labelled) after 1 hour of reaction with buffer B. The scale...
Figure 4: Commercial ZnO sample 3 after treatment with buffer B (2000 mg/L) for one hour. The general appeara...
Figure 5: SiO2-coated labelled ZnO-NP (sample 4; shell thickness 3–6 nm) before (left; scale bar 20 nm) and a...